What Wikipedia says

Pitting corrosion, or pitting, is a form of extremely localized corrosion that leads to the random creation of small holes in metal.

Excerpt from the Wikipedia article “Pitting corrosion”, under the CC BY-SA 4.0 license. Read the article on Wikipedia